316L

UNS S31603

The low carbon variant of 316, having a carbon content less than 0.035%, provides similar corrosion characteristics as 316 and will not form chromium carbides during heating or welding; therefore in many applications post-weld heat treatment is not required. This alloy should not be exposed to prolonged temperatures between 800 °F and 1,500 °F.